Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 454N - PS-I - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 454N:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Styrolution® PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.
Processing/Physical CharacteristicsValueUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 14 cm³/10min ISO 1133
Temperature 200 °C -
Load 5 kg -
Density of melt 935 kg/m³ -
Thermal conductivity of melt 0.165 W/(m K) -
Spec. heat capacity of melt 2290 J/(kg K) -
Ejection temperature 81 °C -
Mechanical propertiesValueUnitTest Standard
ISO Data
Tensile Modulus 2200 MPa ISO 527
Yield stress 27 MPa ISO 527
Yield strain 1.4 % ISO 527
Nominal strain at break 25 % ISO 527
Charpy impact strength, +23°C 150 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 120 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 16 kJ/m² ISO 179/1eA
Thermal propertiesValueUnitTest Standard
ISO Data
Temp. of deflection under load, 1.80 MPa 78 °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 82 °C ISO 75-1/-2
Vicat softening temperature, B 82 °C ISO 306
Coeff. of linear therm. expansion, parallel 100 E-6/K ISO 11359-1/-2
Burning Behav. at 1.5 mm nom. thickn. HB class IEC 60695-11-10
Thickness tested 1.6 mm -
Yellow Card available yes - -
Burning Behav. at thickness h HB class IEC 60695-11-10
Thickness tested 3.2 mm -
Yellow Card available yes - -
Electrical propertiesValueUnitTest Standard
ISO Data
Relative permittivity, 100Hz 2.5 - IEC 62631-2-1
Relative permittivity, 1MHz 2.5 - IEC 62631-2-1
Dissipation factor, 100Hz 1.5 E-4 IEC 62631-2-1
Dissipation factor, 1MHz 4 E-4 IEC 62631-2-1
Other propertiesValueUnitTest Standard
Density 1020 kg/m³ ISO 1183
Test specimen productionValueUnitTest Standard
ISO Data
Injection Molding, melt temperature 220 °C ISO 294
Injection Molding, mold temperature 40 °C ISO 294
Injection Molding, injection velocity 200 mm/s ISO 294
Diagrams
Viscosity-shear rate , Styrolution® PS 454N, PS-I, INEOS Styrolution
Shearstress-shear rate , Styrolution® PS 454N, PS-I, INEOS Styrolution
Stress-strain , Styrolution® PS 454N, PS-I, INEOS Styrolution
Secant modulus-strain , Styrolution® PS 454N, PS-I, INEOS Styrolution
Stress-strain (isochronous) 23°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
Creep modulus-time 23°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
Creep curve 23°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
Stress-strain (isochronous) 40°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
Creep modulus-time 40°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
Creep curve 40°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
Stress-strain (isochronous) 60°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
Creep modulus-time 60°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
Creep curve 60°C, Styrolution® PS 454N, PS-I, INEOS Styrolution
Specific volume-temperature (pvT) , Styrolution® PS 454N, PS-I, INEOS Styrolution
Tensile modulus-temperature , Styrolution® PS 454N, PS-I, INEOS Styrolution
Characteristics
Processing
Injection Molding, Film Extrusion
Delivery form
Pellets
Special Characteristics
High impact or impact modified
Regional Availability
Europe, Near East/Africa
Other text information
Injection molding
PROCESSING
injection molding, Melt temperature, range: 180 - 260 °C
injection molding, Melt temperature, recommended: 220 °C
injection molding, Mold temperature, range: 10 - 60 °C
injection molding, Mold temperature, recommended: 40 °C

Polystyrol 454N can be injection moulded under different conditions depending on machinery available and articles moulded. Mass temperature can be as high as 260°C. Polystyrol 454N is suitable for gas assisted injection moulding. To achieve articles with very high gloss well polished surfaces are recommended.
Film extrusion
PROCESSING
Extrusion, Flat film, Melt temperature: 200 - 240 °C

Extrusion temperatures should not exceed 240°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.